• Stainless Steel SUS 304/304L

Stainless Steel SUS 304/304L

March 11, 2013

SPECIFICATION:

SUS 304

SUS 304L

COMPOSITION: C : MAX 0.08% C : MAX 0.03%
CR : 18 – 20% CR : 18 – 20%
MN : MAX 2% MN : MAX 2%
MO : NIL MO : NIL
NI : 8 – 10% NI : 8 – 12%
P : MAX 0.045% P : MAX 0.045%
S : MAX 0.03% S : MAX 0.03%
SI : MAX 1% SI : MAX 1%
PROPERTIES:
MELTING POINT : 1400 – 1455°C 1400 – 1455°C
SPECIFIC HEAT CAPACITY: 0.5 J/g – °C 0.5 J/g – °C
ELECTRICAL RESISTIVITY @ 20°C : 7.2e – 005 ohm – cm 7.2e – 005 ohm – cm
TENSILE STRENGTH : 500 – 570 MPa 500 – 570 MPa

 

PROFILES

FLAT
HEX
SQUARE
ROUND
PLATE



Comments ( 0 )